?How wide should the test strips be for testing the 10 gauge to 14 gauge thick carbon steel butt, lap, and tee joint welds?

A. ?1 in (25 mm)
B. ?1 ½ (37 mm)
C. ?1/8 in (3 mm)
D. ?3 in (74 mm)


Answer: A

Trades & Technology

You might also like to view...

Does the roof live load vary with occupancy, similar to floor live load?

What will be an ideal response?

Trades & Technology

The _____ organizes the project into detailed tasks and summary tasks.

a. project plan b. materials receiving checklist c. work breakdown structure (WBS) d. organization chart

Trades & Technology

Adding ____ has the same effect on the electrode characteristic as thorium, but is not radioactive.

A. cerium B. lanthanum C. zirconium D. pure tungsten

Trades & Technology

You have been asked to specify criteria for a plastic part that is to be used as a storage tank on a truck that does home lawn fertilizer treatments. What are the most important criteria and why?

What will be an ideal response?

Trades & Technology