A high speed (HSS) lathe tool would have to be above 1300 F. (704 C.) to be overheated. A temperature of 2000 F. (1093 C.) could be produced on the cutting edge when grinding by:
A) Using the roughing wheel for finishing
B) Not cooling it off in water frequently
C) Using a glazed wheel or by forcing the tool into the wheel
D) Using a wheel that is too coarse
C
You might also like to view...
Single-line drawings are always used to show pipe layouts for nominal pipe sizes of less than 12". This is a standard practice for all companies.
Answer the following statement true (T) or false (F)
The ozone layer is located in the layer of the atmosphere called the _______________
Fill in the blank(s) with the appropriate word(s).
Volvo television ads frequently show the company's cars being subjected to crash tests, to
impress consumers with how well-built the cars are and to create the impression that Volvos are among the safest cars on the market. What competitive business strategy does this represent?
a. Differentiation b. Overall cost leadership c. Focus d. Analyzer e. Adaptation
A(n) ____ shows the threads as they appear to the eye.
A. pictorial representation B. simplified representation C. reference representation D. schematic representation