For steels containing more than ____ carbon, preheating and subsequent heat treatment are generally required to produce a satisfactory weld.

A. 0.10%
B. 0.20%
C. 0.30%
D. 0.40%


Answer: D

Trades & Technology

You might also like to view...

The wire sizes used in welded-wire fabric reinforcement are designated by _____.

a. AWG wire gauge b. cross-sectional area in hundredths of a square inch c. cross-sectional area in hundredths of a square centimeter d. diameter in thousandths of an inch

Trades & Technology

The ability of carbon steel to be welded is a function of ____.

A. the melting point B. the ductility C. the welding process D. the carbon content

Trades & Technology

How does green manuring improve the soil?

What will be an ideal response?

Trades & Technology

Technician A says that the torque applied to the head bolts is the same as the clamping force on the gasket. Technician B says that the clamping force is the force actually applied to the surfaces of the gasket. Which technician is correct?

A) Technician A B) Technician B C) Both technicians D) Neither technician

Trades & Technology