The hardness of a supersaturated Al?3% Li?5.5% Mg?0.2% Zr alloy as a function of the aging time and temperature is shown in the following figure.
(a) Describe why at each aging temperature, the hardness goes through a maximum.
(b) Explain why the maximum hardness, and the aging time required for the maximum hardness, increases as the temperature is decreased.
You might also like to view...
On wood-stud and cold-formed steel-stud-wall assemblies, stucco is typically applied in three coats. The total typical thickness of the three coats is ________.
A) 1-1/2 in. B) 1 in. C) 1-1/4 in. D) 1-1/8 in. E) 7/8 in.
For the decision tree branch shown, determine the expected values of the two outcomes if decision D3 is already selected and the maximum outcome value is sought. (This decision branch is part of a larger tree.)
Why is the western flower thrips (Frankliniella occidentalis) considered such a destructive insect pest of greenhouse-grown crops?
What will be an ideal response?
The maximum safe concentration of carbon dioxide (CO2) in an occupied space is _____
a. 900 ppm b. 1,000 ppm c. 1,200 ppm d. 1,500 ppm